Tailoring the textural properties of hierarchical porous carbons for supercapacitors

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

1
2
0

Year Published

2015
2015
2024
2024

Publication Types

Select...
7

Relationship

2
5

Authors

Journals

citations
Cited by 12 publications
(3 citation statements)
references
References 12 publications
1
2
0
Order By: Relevance
“…The leakage current behavior is related to the ash content, the values of leakage current and ash contents follow the same sequence of AC1 < AC3 < AC2. The smaller values of leakage current mean less shuttle reactions caused by the ashes in the activated carbons [21]. The less ash content, the smaller leakage current, which is in according to the results in the literature [12].…”
Section: Electrochemical Propertiessupporting
confidence: 81%
See 1 more Smart Citation
“…The leakage current behavior is related to the ash content, the values of leakage current and ash contents follow the same sequence of AC1 < AC3 < AC2. The smaller values of leakage current mean less shuttle reactions caused by the ashes in the activated carbons [21]. The less ash content, the smaller leakage current, which is in according to the results in the literature [12].…”
Section: Electrochemical Propertiessupporting
confidence: 81%
“…The GCD curves of the activated carbons as electrodes presented in Fig. 5 a exhibit typical triangular shapes without obvious voltage drop at the beginning of discharge, indicating the electrodes have the typical capacitive behaviors [21]. Moreover, the specific capacitances calculated from Eq.…”
Section: Electrochemical Propertiesmentioning
confidence: 92%
“…MC displays a steep uptake below P/P 0 = 0.01 and subsequent saturated adsorption platform, indicating the existence of micropores in large quantity [26,27]. Figure 2(b) shows the pore size distribution (PSD) curves, MG-X display almost the same PSD with the MC's, the pore width range is less than 5 nm, while a remarkable increase happened to the pore volume that the relative pore width range is larger than 5 nm.…”
Section: Resultsmentioning