2018
DOI: 10.1007/s12540-018-0101-z
|View full text |Cite
|
Sign up to set email alerts
|

Three Distinct Deformation Behaviors of Cementite Lamellae in a Cold-Drawn Pearlitic Wire

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1

Citation Types

0
2
0
1

Year Published

2021
2021
2024
2024

Publication Types

Select...
3
1

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(3 citation statements)
references
References 22 publications
0
2
0
1
Order By: Relevance
“…This phenomenon may occur due to projection effects or the large load force during cold drawing process. [ 44 ] More dislocations are formed near the under‐neck region than other areas, with one lattice misfit occurring about every five atomic planes. The lattice spacing of (1,−1,0) ferrite is measured to be 0.211 nm, which is larger than the measured value of 0.206 nm in the initial wire rods.…”
Section: Discussionmentioning
confidence: 99%
See 1 more Smart Citation
“…This phenomenon may occur due to projection effects or the large load force during cold drawing process. [ 44 ] More dislocations are formed near the under‐neck region than other areas, with one lattice misfit occurring about every five atomic planes. The lattice spacing of (1,−1,0) ferrite is measured to be 0.211 nm, which is larger than the measured value of 0.206 nm in the initial wire rods.…”
Section: Discussionmentioning
confidence: 99%
“…As shown in Figure 8a, it can clearly observe a neck-down region (indicated by "B") in the cementite lamella. Xin et al [44] first observed a neck-down region in the partly-broken cementite lamella at an atomic scale. The average thickness of the cementite lamella was measured to be 5.5 AE 0.2 nm, and the smallest In this article, the phenomenon is also observed in the thicker and more complete cementite lamella.…”
Section: Fe/fe 3 C Interface Structure Evolutionmentioning
confidence: 99%
“…Nota-se também a alteração da morfologia da perlita devido à deformação severa. Quando deformado severamente existe a possibilidade de sobressaturar a ferrita do carbono seguindo a tendência do processo de trefilação de aços com microestrutura similar o qual resulta numa região com altíssima resistência (XIN et al, 2018). A Figura 4.17 apresenta a superfície abaixo da superfície de desgaste para a amostra de terceira vida.…”