2019
DOI: 10.1134/s106378261912008x
|View full text |Cite
|
Sign up to set email alerts
|

Ultrasonic-Assisted Exfoliation of Graphitic Carbon Nitride and its Electrocatalytic Performance in Process of Ethanol Reforming

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
12
0

Year Published

2019
2019
2024
2024

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 31 publications
(14 citation statements)
references
References 15 publications
2
12
0
Order By: Relevance
“…Besides, catalytic materials that do not contain expensive metal elements, such as graphite-like carbon nitride or g-C 3 N 4 , have a great potential for development [328]. This catalytic material can be obtained by simple thermolysis of urea, melamine, and other organic precursors in air and exhibits high, stable catalytic characteristics both in the processes of photocatalytic oxidation of organic substances [340,341] and in the electrocatalytic release of hydrogen [342]. FIG.…”
Section: Characteristics and Features Of Methods For The Synthesis Of New Nanostructured Catalystsmentioning
confidence: 99%
“…Besides, catalytic materials that do not contain expensive metal elements, such as graphite-like carbon nitride or g-C 3 N 4 , have a great potential for development [328]. This catalytic material can be obtained by simple thermolysis of urea, melamine, and other organic precursors in air and exhibits high, stable catalytic characteristics both in the processes of photocatalytic oxidation of organic substances [340,341] and in the electrocatalytic release of hydrogen [342]. FIG.…”
Section: Characteristics and Features Of Methods For The Synthesis Of New Nanostructured Catalystsmentioning
confidence: 99%
“…This approach helps increase the phase purity of graphitic carbon nitride powder, decrease its energy band gap, change the morphology, and enhance the material’s specific surface area. For this reason, Chebanenko et al successfully prepared graphitic carbon nitride (g-C 3 N 4 ) by heating 10 g of urea at 550 °C in a quartz tube for 2 h; the resulting material was removed from the tube after cooling [ 9 ]. Subsequently, the material was added to distilled water and stirred for a few minutes with a magnetic stirrer’s aid.…”
Section: Preparation Of Graphitic Carbon Nitride (G-c 3 mentioning
confidence: 99%
“…Subsequently, the material was added to distilled water and stirred for a few minutes with a magnetic stirrer’s aid. The resulting white suspension was exposed to an ultrasonic disintegrator for 2 h. Consequently, the colloidal solution was dried in an oven at 100 °C to remove water molecules and annealed at 300 °C for half an hour to obtain the dry exfoliated g-C 3 N 4 nanopowder [ 9 ].…”
Section: Preparation Of Graphitic Carbon Nitride (G-c 3 mentioning
confidence: 99%
“…The nanopowder of the initial graphitic carbon nitride (g-C 3 N 4 ) was synthesized by heat treatment of urea ((NH 2 ) 2 CO) under aerobic conditions. A detailed description of its synthesis procedure and preparation of a g-C 3 N 4 -based colloidal solution was previously given in [9,10]. After homogenization, 1.5 mg of magnesium acetate tetrahydrate (Mg(CH 3 COO) 2 •4H 2 O or Mg(Ac) 2 •4H 2 O) was dissolved in 10 ml of distilled water using magnetic stirring.…”
Section: Synthesis Proceduresmentioning
confidence: 99%