MnSi layers in Ge-doped MnSi∼1.7 increased with increasing Ge content up to x=0.00133, began to break at x=0.00265 and finally disappeared at x=0.00530. An experimental equation for the growth of MnSi was proposed for the interval between the MnSi layers and amount of doped Ge content. The crystallinity of Ge-doped MnSi∼1.7 increased initially with increasing doped Ge content and saturated at high Ge content. Thermoelectric transport properties along the c-axis of Ge-doped MnSi∼1.7 were measured as a function of Ge content at room temperature. Electrical conductivity and thermoelectric power of Ge-doped MnSi∼1.7 were compared to those of Al-doped MnSi∼1.7 in our previous work. A maximum in the electrical conductivity and a minimum in the thermoelectric power of Ge-doped MnSi∼1.7 were observed at x=0.00133, reflecting a change in hole density which was influenced by the volume ratio of MnSi. Hole mobility depended on the existence of MnSi layers and/or of interfaces between MnSi∼1.7 and MnSi and on the crystallinity of MnSi∼1.7. The thermal conductivity of Ge-doped MnSi∼1.7 had a maximum at x=0.00053. The increase in thermal conductivity at low Ge doping can be explained by the increase in the amount of MnSi segregated in doped MnSi∼1.7, while the decrease at high Ge content was caused by the increase in phonon scattering of Ge. A maximum figure of merit of Ge-doped MnSi∼1.7 was obtained at x=0.00974, reflecting a maximum power factor.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.