Beginning‐of‐life H
2
‐fed fuel cell performance of membrane electrode assemblies (MEA) made using state‐of‐the‐art subcomponents (25–50 µm membranes, 47 wt% Pt on carbon, 0.15–0.4 mg cm
−2
Pt cathode loading, ≤1100 equivalent weight (EW) ionomer/binder) was studied. Performance data were taken using small‐scale (50 cm
2
) cells and a large‐scale (500 cm
2
, 22 cell) stack, and voltages were corrected for membrane resistance in order to isolate cathode polarization losses. Based on catalyst and MEA cyclic voltammetry and in‐situ testing with pure O
2
feed, we observed loading independent O
2
kinetic control up to 1.8 A cm
−2
at 80 °C under fully humidified conditions; this indicates negligible effects of cathode layer proton transport limitations with pure O
2
. With air as the oxidant, we observed O
2
kinetic control below 0.2 A cm
−2
and the onset of O
2
transport resistances at higher current densities. Results with helox (21% O
2
in helium) as the cathode feed revealed that the O
2
transport resistances were roughly evenly distributed between gas and solid phases. With incomplete reactant humidification, additional membrane resistance was observed and proton conductivity losses in the cathode layer became significant. Moreover, thin (25 µm) low‐equivalent weight (EW) MEAs outperformed thicker (50 µm) high EW MEAs even after correcting for membrane ohmic losses. This is due to faster water transport of the thinner low EW MEAs resulting in improved retention of cathode layer proton conductivity under dry conditions.
Membrane failures at catalyst layer edges in proton exchange membrane fuel cell ͑PEMFC͒ membrane electrode assemblies ͑MEAs͒ were investigated using MEAs with segmented electrodes. A mathematical model was developed to predict the potential distribution at the edge of the MEA with misaligned electrodes. Control experiments were performed using an accelerated membrane durability test protocol and significant membrane degradation was observed in the region where the cathode overlaps the anode. The model-experiment comparisons suggest that a high cathode potential contributes to the membrane failure. A dependence of membrane degradation on relative humidity ͑RH͒ was observed in the experiments, regardless of the electrode overlap. The observed membrane degradation in the overlap region of MEAs with an anode catalyst overlap, run at low RH, is not explained by the model and needs further investigation.
Adsorbed CO Stark tuning rates have been studied for the first time in direct methanol fuel cells on Pt black
catalysts supported only on the polymer electrolyte (Nafion) in membrane electrode assemblies. The bipolar
peaks resulting from the Stark shift of CO absorbance peaks are inverted, indicating an anomalous increase
in the reflectivity where CO infrared absorption occurs. The vibrational Stark tuning data suggests that CO
oxidation occurs on the perimeter of COads islands, which is consistent with the formation of CO within and
above Pt double layer potentials as reported by Kunimatsu. This is expected since methanol is continuously
delivered to the anode at all potentials in direct methanol fuel cells.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.