Objective: To evaluate the Vickers hardness of different acrylic resins for denture bases with and without the addition of glass fibres. Background: It has been suggested that different polymerisation methods, as well as the addition of glass fibre (FV) might improve the hardness of acrylic. Materials and methods: Five types of acrylic resin were tested: Vipi Wave (VW), microwave polymerisation; Vipi Flash (VF), auto-polymerisation; Lucitone (LT), QC20 (QC) and Vipi Cril (VC), conventional heat-polymerisation, all with or without glass fibre reinforcement (GFR) and distributed into 10 groups (n = 12). Specimens were then submitted to Vickers hardness testing with a 25-g load for 30 s. All data were submitted to ANOVA and Tukey's HSD test. Results: A significant statistical difference was observed with regard to the polymerisation method and the GFR (p < 0.05).
Endomethasone interfered negatively with the bond to root dentine; however, AH Plus, Epiphany and Sealer 26 did not interfere in the bond strength of a fibreglass post cemented with self-adhesive resin cements.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.