Strontium titanate SrTiO 3 (100), (110), and (111) single crystals, undoped or donor doped with up to 1 at% La, were isothermally equilibrated at temperatures between 1523 and 1773 K in synthetic air followed by two different methods of Sr tracer deposition: ion implantation of 87 Sr and chemical solution deposition of a thin 86 SrTiO 3 layer. Subsequently, the samples were diffusion annealed under the same conditions as before. The initial and final depth profiles were measured by SIMS. For strong La-doping both tracer deposition methods yield similar Sr diffusion coefficients, whereas for weak doping the tracer seems to be immobile in the case of ion implantation. The Sr diffusivity does not depend on the crystal orientation, but shows strong dependency on the dopant concentration supporting the defect chemical model that under oxidizing conditions the donor is compensated by Sr vacancies. A comparison with literature data on Sr vacancy, Ti, and La diffusion in this system confirms the concept that all cations move via Sr vacancies. Cation diffusion is several orders of magnitude slower than oxygen diffusion.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.