Polyimides having long poly(ethylene oxide), PEO, moieties in the main chain have been synthesized by a classical two-steps polycondensation method with good yield and high molecular weight. In contrast with previous works on this topic, essentially full conversion of the polyamic acid to polyimide was attained by heating at relatively low temperatures (around 160 ºC). These copolyimides undergo an increase of phase separation between the PEO part and the polyimide one after a thermal annealing. This phase separation increases gas separation properties of membranes made up of these copolymers. An exhaustive study of polymer properties as a function of the thermal treatment has been carried out in order to figure out the origin of this behavior. The analysis performed included TGA, DSC, SAXS and mechanical testing. The polymers studied in this paper have medium thermal stability. In fact, degradation of the polyether chain under nitrogen takes place at temperatures above 300 ºC. However, their thermal stabilities were much lower under oxidant atmosphere.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.