The glancing angle deposition (GLAD) technique is used to fabricate nanostructured thin films with high surface area. Quantifying this property is important for optimizing GLAD-based device performance. Our group has used high-sensitivity krypton gas adsorption and the complementary technique of cyclic voltammetry to measure surface area as a function of deposition angle, thickness, and morphological characteristics for several metal oxide thin films. In this work, we studied amorphous titanium dioxide (TiO(2)), amorphous silicon dioxide (SiO(2)), and polycrystalline indium tin oxide (ITO) nanostructures with vertical and helical post morphologies over a range of oblique deposition angles from 0 to 86 degrees. Krypton gas sorption isotherms, evaluated using the Brunauer-Emmettt-Teller (BET) method, revealed maximum surface area enhancements of 880 +/- 110, 980 +/- 125, and 210 +/- 30 times the footprint area (equivalently 300 +/- 40, 570 +/- 70, and 50 +/- 6 m(2) g(-1)) for vertical posts TiO(2), SiO(2), and ITO. We also applied the cyclic voltammetry technique to these ITO films and observed the same overall trends as seen with the BET method. In addition, we applied the BET method to the measurement of helical films and found that the surface area trend was shifted with respect to that of vertical post films. This revealed the important influence of the substrate rotation rate and film morphology on surface properties. Finally, we showed that the surface area scales linearly with film thickness, with slopes of 730 +/- 35 to 235 +/- 10 m(2) m(-2) microm(-1) found for titania vertical post films deposited at angles from 70 to 85 degrees. This characterization effort will allow for the optimization of solar, photonic, and sensing devices fabricated from thin metal oxide films using GLAD.
A new growth technique for indium tin oxide nanowhiskers with increased control over feature size and spacing is reported. The technique is based on a unique combination of self-catalysed vapour-liquid-solid (VLS) growth and glancing angle deposition (GLAD). This VLS-GLAD technique provides enhanced control over nanowhisker morphology as the effect of typical VLS growth parameters (e.g. flux rate, temperature) is amplified at large deposition angles characteristic of GLAD. Spatial modulation of the collimated growth flux controls trunk width, number and orientation of branches, and overall nanowhisker density. Here we report the influence of growth conditions (including deposition angle, flux rate, nominal pitch and substrate temperature) on nanowhisker morphology, with specific focus on the effect of large deposition angles. Sheet resistance and transmission of the films were measured to characterize their performance as transparent conductive oxides. Hybrid nanostructured films grown in this study include high surface area nanowhiskers protruding from a conductive film, ideal for transparent conductive electrode applications.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.