In order to investigate the failure behavior of fuel cladding under a reactivity-initiated accident (RIA) condition, biaxial stress tests on unirradiated Zircaloy-4 cladding tube with an outer surface pre-crack were carried out under room temperature conditions by using an improved Expansion-Due-to-Compression (improved-EDC) test method which was developed by Japan Atomic Energy Agency. The specimens with an outer surface pre-crack were prepared by using Rolling-After-Grooving (RAG) method. In each test, a constant longitudinal tensile load of 0, 5.0 or 10.0 kN was applied along the axial direction of specimen, respectively. All specimens failed during the tests, and the morphology at the failure opening of the specimens was similar to that observed in the result of post-irradiation examinations of high burnup fuel which failed during a pulse irradiation experiment. The longitudinal strain (ε tz ) at failure clearly increased with increasing longitudinal tensile loads and the circumferential strain (ε tϑ ) at failure significantly decreased in the case of 5.0 and 10.0 kN tests, compared with the case of 0 kN tests. From these tests, the data of cladding failure were obtained in the range of strain ratio (ε tz /ε tϑ ) between about −0.6 and 0.7: this range of strain ratio covers the range between about 0.0 and 0.7 which is estimated in the case of RIAsimulated test. It is considered that the data obtained in this study can be used as a fundamental basis for quantifying the failure criteria of fuel cladding under a biaxial stress state.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.