A detailed study
of the sedimentation kinetics of iron oxide nanoparticle
(IONP) clusters composed of nanospheres and nanorods is presented.
Measurements were performed to determine the absorbance of an IONP
suspension undergoing sedimentation over time by using a UV–vis
spectrophotometer with simultaneous monitoring of the hydrodynamic
diameter of the clusters formed with dynamic light scattering (DLS).
Mathematical analysis based on Happel’s spherical and cylindrical
models was conducted to reveal the relationship between the settling
velocity of the IONP clusters and their packing density. For the case
of IONP clusters composed of rodlike particles, two distinctive phases
of sedimentation were recorded, with the occurrence of rapid sedimentation
at the beginning of the process (phase I) followed by a slower settling
rate (phase II). In sedimentation phase II, even though the nanorod
clusters had a hydrodynamic size of >500 nm, which was much larger
than that of the nanosphere clusters (∼200 nm), their settling
velocity of 0.0038 mm/min was still slower than that of the nanosphere
clusters. Such observations were mainly a result of the packing density
differences between the formed clusters; due to the end-to-end particle
interactions of nanorods, the nanorod clusters were less tightly packed
and more permeable. In addition to the mathematical analysis, quartz
crystal microbalance with dissipation (QCM-D) was employed to measure
the “softness” of the IONP clusters formed, and this
physical property can be further related to their packing density.
This study illustrated that for a rapidly aggregating system, such
as magnetic IONPs, not only do the particle shape and size uniformity
contribute to the physical properties of the particle clusters formed
but also the nature of the aggregation, either end-to-end and/or side-to-side,
should be carefully considered when designing a colloidally stable
IONP suspension.
To evaluate the growth rate of larval and pupal parameters of silkworm Bombyx mori fed with Silver Nanoparticles (AgNps) treated MR 2 mulberry leaves, the following works have been considered. The AgNp was synthesized by chemical reduction method, it was diluted by different concentrations such as 25%, 50%, 75% and 100% (without dilution). Fresh mulberry leaves (Morus alba L.) were sprayed by each concentration and were fed to silkworms, from 3 rd , 4 th and 5 th instar, five feedings/day. Group T 1 larvae received MR 2 mulberry leaves sprayed with distilled water and served as control, group T 2 , T 3 , T 4 and T 5 larvae received 25%, 50%, 75% and 100% AgNps sprayed mulberry leaves, respectively. Silkworm larvae fed on M. alba (MR 2 ) leaves sprayed with 25% concentration of AgNps (group T 2 ) was significantly increased the larvae and cocoon length, width and weight as compared to those fed on control (group T 1 ) MR 2 mulberry leaves and other groups (T 3 , T 4 and T 5 ). Hence, 25% AgNps dose was fixed as an effective dose. It has been observed from the present study that 25% AgNps treated (group T 2 ) leaves fed by silkworms have enhanced the larval and pupal growth and quantity of silk production than control.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.