“…3,5 But, the VHB tape shows low electrical breakdown strength (E b , z30 kV mm À1 ) and high viscoelastic loss, which limits w max , power conversion efficiency (PCE) and fatigue life (N FL ) of the DEG. Up to now, many kinds of DE materials such as silicone rubber (SiR), [6][7][8][9][10][11] polyurethane (PU), [12][13][14] natural rubber (NR) 15 and poly(styrene-butadiene-styrene) (SBS) 16 have been employed as DEG materials for replacing the VHB tape. Among these materials, SiR is one of the most promising materials for the practical application of DEG due to its high electrical insulation, high E b (z60 kV mm À1 ), high elasticity and low elastic modulus (Y).…”