Dimensional variation in production of high-aspect-ratio micro-pillars array by micro powder injection molding

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
22
0

Year Published

2010
2010
2019
2019

Publication Types

Select...
4
4

Relationship

0
8

Authors

Journals

citations
Cited by 21 publications
(22 citation statements)
references
References 16 publications
0
22
0
Order By: Relevance
“…Due to the effect of smaller powder size, the temperature profile of debinding and sintering in PIM are controlled strictly to avoid the occurrence of warpage, bubble and contamination. The surface roughness, shrinkage, microstructure, micro-mechanical and micro-tribologoical properties of microcomponents were characterized by various methods [10][11][12][13]. These results, in turn, can optimize the processing parameters of PIM.…”
Section: Introductionmentioning
confidence: 99%
“…Due to the effect of smaller powder size, the temperature profile of debinding and sintering in PIM are controlled strictly to avoid the occurrence of warpage, bubble and contamination. The surface roughness, shrinkage, microstructure, micro-mechanical and micro-tribologoical properties of microcomponents were characterized by various methods [10][11][12][13]. These results, in turn, can optimize the processing parameters of PIM.…”
Section: Introductionmentioning
confidence: 99%
“…A detailed analysis of the influence of the injection 13.3 Tooth brackets made of Ni-free steel alloy (courtesy of Bernhard Fö rster GmbH, Pforzheim, Germany). molding parameters on the precision of the molded parts is given, for example, in (Billiet, 1985;Zauner et al, 2004;Greene and Heaney, 2007;Li et al, 2007;Beck et al, 2008;. Depending on the powder particle sizes and filling rates, the reproducibility of component dimensions is ±0.3 to ±0.5% for metals, ±0.5% for alloyed powders, and ±0.2 to ±0.5% for ceramics.…”
Section: Micro Powder Injection Molding (Micropim) -Molding Proceduresmentioning
confidence: 97%
“…Within the process chain of μPIM, the three main processes of injection moulding, debinding and sintering take place in a high pressure and/or high temperature environment. Therefore, significant variation in some key parameters, such as volume and warpage, are expected [24].…”
Section: Shape Deformation In μPimmentioning
confidence: 99%
“…With regards to part volume, dimensions typically decrease by about 2% after moulding, but some reported research indicated the possibility of post-moulding dimensional decrease by approximately 6% [24]. Another 15% decrease in dimensions might result after sintering.…”
Section: Shape Deformation In μPimmentioning
confidence: 99%
See 1 more Smart Citation