2017
DOI: 10.19182/bft2016.330.a31318
|View full text |Cite
|
Sign up to set email alerts
|

Effects of Nano-Silane on the Physical and Mechanical Properties of Oriented Strand Lumber (Osl)

Abstract: Cette étude s'est penchée sur les effets de la teneur en résine et en composés de nano-silane (NS) sur les panneaux structuraux orientés (OSB), un important produit en bois reconstitué. Des panneaux OSB ont été fabriqués avec de la résine d'urée-formaldéhyde (UF) à 8 % et à 10 % (sur poids sec des panneaux), avec application de NS à deux teneurs en fonction de la teneur en résine UF. Nos résultats montrent que les traitements aux deux teneurs différentes en résine donnent des valeurs très proches pour les modu… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

0
4
0

Year Published

2018
2018
2022
2022

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 6 publications
(4 citation statements)
references
References 15 publications
0
4
0
Order By: Relevance
“…At this resin content, it seems that nanowollastonite caused poor wetting of wood strips since the majority of failures were due to the resin and not to the wood. Another possible explanation for this behavior may be the absorption or gathering of resin molecules by wollastonite nanofibers, preventing them from being active in the process of sticking the strips together [39,40,41].…”
Section: Resultsmentioning
confidence: 99%
“…At this resin content, it seems that nanowollastonite caused poor wetting of wood strips since the majority of failures were due to the resin and not to the wood. Another possible explanation for this behavior may be the absorption or gathering of resin molecules by wollastonite nanofibers, preventing them from being active in the process of sticking the strips together [39,40,41].…”
Section: Resultsmentioning
confidence: 99%
“…Although in industrial practice the shape of wood particles is irregular, except for veneerbased materials, they are still described by linear dimensions of a parallelepiped. For wood particles used to manufacture OSL in laboratory conditions, linear dimensions are within the following ranges: 78 mm to 142 mm long, 9 mm to 60 mm wide, and 0.55 mm to 0.75 mm thick (Preechatiwong et al 2007;Beck et al 2009;Taghiyari et al 2016). Generally, the material used in the studies is of a uniform size fraction, and the thickness of the manufactured boards is less than 20 mm, mainly due to technical limitations.…”
Section: Introductionmentioning
confidence: 99%
“…Addition of Cloisite 30B resulted in significant improvement in mechanical properties of wood polymer composites (Samariha et al, 2015). However there is report of compactness of strips having more effect on oriented strand lumber when prepared with different concentration of UF resin along with nano-silane (Taghiyari et al, 2016a). One of the ways to decrease the formaldehyde emission of the UF boned panels is to use nano-fillers such as nanoclay and nano-SiO 2 because these materials have strong absorbability as well as high barrier property (Roumeli et al, 2012).…”
Section: Introductionmentioning