Enhancing the anti-oxidation stability of vapor-crystallized arsenic crystals via introducing iodine

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2023
2023
2024
2024

Publication Types

Select...
4

Relationship

1
3

Authors

Journals

citations
Cited by 4 publications
(2 citation statements)
references
References 43 publications
0
2
0
Order By: Relevance
“…There is no obvious difference between the surface and cross-section morphology, and it can be seen that with the increase of the supercooling degree, the XRD diffraction peaks of the product arsenic become smaller and smaller, and it gradually transforms from the crystalline state to the amorphous state. ; As grows along the (021) direction at 623 K, which is different from the growth of the parent material along the (003) direction, which is related to the pressure of the system during the growth process [29]. The temperature above 623 K shows a staggered, stepped, multifaceted surface, which is typical of crystalline As, and its growth mode is laminar growth.…”
Section: Results Of the Experimentsmentioning
confidence: 99%
“…There is no obvious difference between the surface and cross-section morphology, and it can be seen that with the increase of the supercooling degree, the XRD diffraction peaks of the product arsenic become smaller and smaller, and it gradually transforms from the crystalline state to the amorphous state. ; As grows along the (021) direction at 623 K, which is different from the growth of the parent material along the (003) direction, which is related to the pressure of the system during the growth process [29]. The temperature above 623 K shows a staggered, stepped, multifaceted surface, which is typical of crystalline As, and its growth mode is laminar growth.…”
Section: Results Of the Experimentsmentioning
confidence: 99%
“…The highly oriented b-AsP is thoroughly exposed with the (010) facet exhibiting the minimum surface energy, which has much lower chemical reaction activity with oxygen. 41,42 In comparison, the b-AsP-Control sample has large amounts of other Miller index facets exposed to ambient conditions, and it would lead to higher oxidation reaction activity since these facets have higher surface energy.…”
Section: Highly Oriented Exfoliated B-asp Flakesmentioning
confidence: 99%