Impact of crystallization on ferro-, piezo- and pyro-electric characteristics in thin film P(VDF–TrFE)

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
31
0

Year Published

2017
2017
2024
2024

Publication Types

Select...
9

Relationship

0
9

Authors

Journals

citations
Cited by 46 publications
(34 citation statements)
references
References 27 publications
2
31
0
Order By: Relevance
“…These results are consistent with the observations made by Choi et al . for thick multi‐layer Langmuir–Blodgett films and spin coated bulk P(VDF‐TrFE) films . This dilation of d spacing is prominent in P(VDF‐TrFE) rich melt‐mixed blends.…”
Section: Resultssupporting
confidence: 92%
“…These results are consistent with the observations made by Choi et al . for thick multi‐layer Langmuir–Blodgett films and spin coated bulk P(VDF‐TrFE) films . This dilation of d spacing is prominent in P(VDF‐TrFE) rich melt‐mixed blends.…”
Section: Resultssupporting
confidence: 92%
“…For example, a low T c of 105 C was measured for a copolymer of 70/30 composition ratio. 88 A previous study 89 demonstrated that T c is 70-80 C for a 65/ 35 mol% P(VDF-co-TrFE) copolymer, which was observed as a decrease in the intensity of the XRD diffraction peak at 2q ¼ 19.5 (b-phase), and the emergence of a second peak at 2q ¼ 18.2 (a-phase) as the temperature increased above 80 C. The all-trans peak vanished at 100 C (lower than the melting temperature, T m $ 153 C). In the temperature between T c and T m , the polymer chains move more freely to reorganise into higher degree of crystallinity.…”
Section: Structure Of Polyvinylidene Uoride (Pvdf) and Polymorphsmentioning
confidence: 99%
“…For a P(VDF-co-TrFE) copolymer with a composition ratio of 72.2/27.8 mol%, 88 the polymer chain length affects the conformations. It was found that a short polymer chain length leads to a higher crystal size and promotes a higher b-phase content; the d 33 piezoelectric coefficient was enhanced by decreasing the molecular weight (M w ) of the copolymer.…”
Section: Structure Of Polyvinylidene Uoride (Pvdf) and Polymorphsmentioning
confidence: 99%
“…After each deposition, the layer is annealed for 15 min at 135 • C in an infrared oven. It allows the solvent to evaporate and the PVDF-TrFE film to crystallize [11].…”
Section: Electro-active Polymermentioning
confidence: 99%