2017
DOI: 10.17973/mmsj.2017_02_2016190
|View full text |Cite
|
Sign up to set email alerts
|

MECHANICAL PROPERTIES AND POROSITY OF Ti-6Al-4V ALLOY PREPARED BY AM TECHNOLOGY

Abstract: Efficient machining using wire electrical discharge machining (WEDM) technology is a compromise between cutting speed and resulting surface quality. Typical morphology of the surface machined by WEDM shows a plenty of craters caused by electrospark discharges produced during the cutting process. This work is focused on assessing the impact of machine setting parameters on quantitative and qualitative evaluation of the workpiece surface of aluminium alloy AlZn6Mg2Cu. Using metallography, the surface effects ari… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
4
1

Citation Types

0
8
0

Year Published

2017
2017
2023
2023

Publication Types

Select...
9

Relationship

1
8

Authors

Journals

citations
Cited by 11 publications
(8 citation statements)
references
References 0 publications
0
8
0
Order By: Relevance
“…Previous publications studied the mechanical properties of metallic SLM parts, including 316 stainless steel [10,11], Ti6Al4V [12][13][14][15], Inconel 718 [16] and aluminum alloys [3][4][5][6][7][8][9][17][18][19][20][21][22][23][24][25][26][27][28].…”
Section: Introductionmentioning
confidence: 99%
“…Previous publications studied the mechanical properties of metallic SLM parts, including 316 stainless steel [10,11], Ti6Al4V [12][13][14][15], Inconel 718 [16] and aluminum alloys [3][4][5][6][7][8][9][17][18][19][20][21][22][23][24][25][26][27][28].…”
Section: Introductionmentioning
confidence: 99%
“…The only possible answer for these boundary conditions is additive manufacturing technology. The powder of Ti6Al4V alloy is most commonly processed by direct metal laser sintering (DMLS) and selective laser melting (SLM) [1][2][3][4][5][6][7][8][9][10][11].…”
Section: Introductionmentioning
confidence: 99%
“…No internal defects, discontinuities, or large irregular pores are visible on the OM images. Porosity below 0.1% has almost no effect on the resulting mechanical properties [8,11,47,[50][51][52]. The pores that were detected and analyzed were characterized by an optimal spherical shape without significant sharp edges.…”
Section: Microstructure Analysis Of the As-built Samplesmentioning
confidence: 99%