2017
DOI: 10.1016/j.jallcom.2016.12.086
|View full text |Cite
|
Sign up to set email alerts
|

Microanalysis of crystallographic characteristics and structural transformations in SPDed Al Mn Si alloy by dual-straining

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
9
0

Year Published

2017
2017
2021
2021

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 76 publications
(9 citation statements)
references
References 14 publications
0
9
0
Order By: Relevance
“…The grains in the WZ of the laser beam welded joint have stronger diffraction peaks and smaller half-width in the crystal index of 1012 À Á , 1110 À Á and 1013 À Á indicating a coarser grain size. Meanwhile, the diffraction peaks of the laser-MIG hybrid welds slightly shifted to the right, suggesting that there was a considerable extent of internal stress or lattice distortion in the joint [32]. This large stress or lattice distortion can be related to the formation of twins in the welded joints.…”
Section: X-ray Diffractionmentioning
confidence: 97%
“…The grains in the WZ of the laser beam welded joint have stronger diffraction peaks and smaller half-width in the crystal index of 1012 À Á , 1110 À Á and 1013 À Á indicating a coarser grain size. Meanwhile, the diffraction peaks of the laser-MIG hybrid welds slightly shifted to the right, suggesting that there was a considerable extent of internal stress or lattice distortion in the joint [32]. This large stress or lattice distortion can be related to the formation of twins in the welded joints.…”
Section: X-ray Diffractionmentioning
confidence: 97%
“…28 Variation in micro strain and dislocation line density in terms of ion dose are shown in the Figures 5 and 6, respectively, for all the three planes. 29 In both Figures 5 and 6, plane (1 1 1) and plane (2 0 0), abrupt changes occur at the initial ion doses, but behavior of plane (2 0 0) strain increases in start and at the final ion dose, all the planes value comes closer in the end.…”
Section: Resultsmentioning
confidence: 85%
“…The XRD graph confirms that the intensity of the diffraction lines of Figure 5 c is decreased with a larger width when compared to other Zn composites (0.5 g/L) and pure Zn coating. Williamson-Hall and Sherrer’s method can be applied to determine the crystallite size [ 4 , 70 ]. The present work used the Sherrer’s method to determine the average crystal size of deposits as plated Zn and Zn–WO 3 composites (Equation (1)).…”
Section: Resultsmentioning
confidence: 99%