“…The resultant slurry was ultrasonically vibrated with heptane solvent and settled down for 10 min, during which the nanoflakes sediment were separated from the small nanoparticles [6][7][8]. The flakes were then coated with iron nanoparticles by sono-chemical method [9], and the nominal a-Fe content was 0-10 wt.%. The hybrid SmCo 5 /a-Fe powers were magnetically aligned and then sintered at 650°C for 5 min under 300 MPa by spark plasma sintering method.…”