2018
DOI: 10.1016/j.cirp.2018.04.082
|View full text |Cite
|
Sign up to set email alerts
|

Study of an annular laser beam based axially-fed powder cladding process

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
15
0

Year Published

2019
2019
2023
2023

Publication Types

Select...
7

Relationship

1
6

Authors

Journals

citations
Cited by 32 publications
(15 citation statements)
references
References 8 publications
0
15
0
Order By: Relevance
“…The catchment efficiency of powders generally depends on the feed rate of powders, the flow rate of carrier gas, the diameter distribution of powders, the beam profile of the laser, the scan speed of the laser, etc. [42,72,94]. Despite the maximum catchment efficiency of powders was reported to be nearly 90% for a specific case, the material usage efficiency of LAM-DED process is generally less than 30% [42,57,74].…”
Section: Effects Of Deposition Parametersmentioning
confidence: 99%
See 2 more Smart Citations
“…The catchment efficiency of powders generally depends on the feed rate of powders, the flow rate of carrier gas, the diameter distribution of powders, the beam profile of the laser, the scan speed of the laser, etc. [42,72,94]. Despite the maximum catchment efficiency of powders was reported to be nearly 90% for a specific case, the material usage efficiency of LAM-DED process is generally less than 30% [42,57,74].…”
Section: Effects Of Deposition Parametersmentioning
confidence: 99%
“…5 [42,[57][58][59][60][94][95][96][97]. The power of the laser, the scan speed of the laser and the feed rate (mass flow rate) of powders are major parameters affecting the bead formation, joining between successive layers, the porosity, the microstructure, and the residual stress [42,60,98].…”
Section: Effects Of Deposition Parametersmentioning
confidence: 99%
See 1 more Smart Citation
“…1(a), consists of an ALB-DWD head, a wire-feeding unit, a workpiece translation stage, a process-monitoring system and a continuous, 2.5-kW, fiber laser source with a wavelength of 1080 nm. Using a laser beam shaping unit in the ALB-DWD head [8,9], a collimated laser beam is transformed into an ALB. By means of two reflective mirrors, the ALB is guided coaxially to the axis of the wire-guiding tube and focused on the workpiece surface using focusing optics.…”
Section: Annular Laser Beam Wire-deposition Setup and Wipmentioning
confidence: 99%
“…Laser cladding is a coating technology that deposits multiple layers of composite material on the substrate to improve the physical properties of the work-piece such as wear resistance and corrosion resistance [1][2][3][4] . Laser cladding technology is widely used in surface enhancement and wear repair of parts [5][6][7][8][9] .…”