2015
DOI: 10.1080/15685551.2015.1070505
|View full text |Cite
|
Sign up to set email alerts
|

Synthesis and characterization of polyurethane-urea-amide based on functionalized polystyrene

Abstract: Hexamethylene diisocyanate (HMDI) based polyurethane-urea-amide (PUUA) is synthesized using diamide chain extenders and dihydroxy polystyrene. The rigid segment structure is HMDI-6X6-HMDI. The repeating molecular weight of the soft segment is varied from 2678 to 9202 g mol −1 using HMDI as a chain extender. The inherent viscosity of the polymer is 1.3-3.9 dL g −1 . Tm of PUUA varies between 239 and 265°C. The crystallinity of the amide segments is up to 70%. The polymers show single-stage decomposition tempera… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
7
0

Year Published

2018
2018
2023
2023

Publication Types

Select...
5

Relationship

0
5

Authors

Journals

citations
Cited by 5 publications
(7 citation statements)
references
References 22 publications
0
7
0
Order By: Relevance
“…The Tg obtained at crosslinked samples which contain the same low DATA amount (DT2, DT5, DT6) is around −54 C. This emphasizes the strong influence of the DATA structure on the structure of the hard domain, through its volume and rigidity, as well as the importance of strong hydrogen bonds, which ensure a stronger ordering of the microphases. 39…”
Section: Resultsmentioning
confidence: 99%
“…The Tg obtained at crosslinked samples which contain the same low DATA amount (DT2, DT5, DT6) is around −54 C. This emphasizes the strong influence of the DATA structure on the structure of the hard domain, through its volume and rigidity, as well as the importance of strong hydrogen bonds, which ensure a stronger ordering of the microphases. 39…”
Section: Resultsmentioning
confidence: 99%
“…The amorphous and crystalline amide peak height (h) are related by the factor “C” which is having the value of 2.4. 23…”
Section: Methodsmentioning
confidence: 99%
“…The inherent viscosity of the synthesized polymer at a strength of 0.1 dL/g in a 1:1 molar solution of phenol/1,1,2,2-tetrachloroethane is found at 25°C by capillary Ubbelohde by adopting the known procedure. 23…”
Section: Methodsmentioning
confidence: 99%