Aluminium and copper plates with 3 mm thickness were successfully friction stir lap welded at a lower rotation rate of 600 rev min 21 using a larger pin 8 mm in diameter. Good metallurgical bonding on the Al/Cu interface was achieved due to the formation of a thin, continuous and uniform Al-Cu intermetallic compound layer. Furthermore, many Cu particles consisting of pure Cu and intermetallic compound layers were generated at the lower part of the nugget zone, forming a composite structure with increased hardness. A lower rotation rate resulted in a decrease in annealing softening in the heat affected zone (HAZ), and a larger diameter pin increased the Al-Cu bonding area. These factors resulted in that the friction stir welded lap joint exhibited a high failure load of 2680 N with failure in the HAZ on the aluminium side.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.