2017
DOI: 10.1063/1.4983772
|View full text |Cite
|
Sign up to set email alerts
|

Characterization methodology for lead zirconate titanate thin films with interdigitated electrode structures

Abstract: The accurate evaluation of ferroelectric thin films operated with interdigitated electrodes is quite a complex task. In this article, we show how to correct the electric field and the capacitance in order to obtain identical polarization and CV loops for all geometrical variants. The simplest model is compared with corrections derived from Schwartz-Christoffel transformations, and with finite element simulations. The correction procedure is experimentally verified, giving almost identical curves for a variety … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

0
32
0

Year Published

2017
2017
2025
2025

Publication Types

Select...
7
1
1

Relationship

0
9

Authors

Journals

citations
Cited by 22 publications
(32 citation statements)
references
References 20 publications
0
32
0
Order By: Relevance
“…as shown in [24]. Similar to reference [30], the total electric charge per unit width on an electrode of the IDE cantilever can be found from Gauss' law by integrating the normal component of the electric displacement vector around a contour as shown in Fig. 4 and summing over all fingers of the electrode.…”
Section: K Smentioning
confidence: 91%
“…as shown in [24]. Similar to reference [30], the total electric charge per unit width on an electrode of the IDE cantilever can be found from Gauss' law by integrating the normal component of the electric displacement vector around a contour as shown in Fig. 4 and summing over all fingers of the electrode.…”
Section: K Smentioning
confidence: 91%
“…Reference samples made of sputtered 100-nm-thick Pt electrodes with the same IDE design were also realized by standard lithography/ion beam etching process. The absolute values of electric field E , relative dielectric permittivity ε ’ and polarization P were extracted from the measurements as recently described by Nigon et al [ 16 ]. Because the gap and width of the fingers are significantly larger than the thickness of the film ( a , b >> t f ), the effective gap a + Δ a (Δ a = 1.324 × t f ) was used in the calculations.…”
Section: Methodsmentioning
confidence: 99%
“…This configuration avoids using the bottom electrode, thus facilitating the substrate's choice with desired lattice mismatch (and therefore biaxial strain). 29 The sinusoidal electric field was generated by AIM-TTI TGP 3100 function generator, amplified by a…”
Section: Online Contentmentioning
confidence: 99%